MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Danquinsa DANCURE® 101 Isocyanate Hardeners
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANCURE® 101 is based on aliphatic Polyisocyanate and doesn’t contain any solvent. DANCURE® 101 is water soluble and can be used as a crosslink for all water based PUR- and polymer dispersions, polyvinyl acetate, Hydroxyl functional polymer’s, for Industrial 2-Components, aqueous PUR-Coatings and wood finishes. Properties:
  • Fast cross linking
  • High reactive, high initial tensile strengths
  • No discolouration
  • Good water solubility
  • High thermal stability.
  • Increases the resistance of bonding films to
  • greases, plasticiser, water and various solvents.
Application: The adhesive-dispersion must be mixed with DANCURE® 101 thoroughly to get a good homogenization otherwise it can lead to granular deposits. The hardener-adhesive mixture must be processed within pot life. Water based systems don’t start gelling after pot life is finished. End of pot life (lasts for several hours) can be determined by decrease of strength of the bond. After adding DANCURE® 101 again one can achieve the original strength of bond again.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³DIN 51.757
Solids Content 100 %100 %DIN 53.1
Brookfield Viscosity 2100 - 2500 cP2100 - 2500 cPSpindle IV, 20 rpm
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Chemical compositionAliphatic Polyisocyanate
Composition<0.3%Free monomer
 21-23%NCO (as supplied)
Physical formClear, liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ105 / 294525

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.