MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Extra-high-leaded brass, UNS C35600, H01 sheet/strip
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Fair to excellent corrosion resistance. Excellent machinability. Fabricated by blanking, machining, piercing and punching, stamping.

Applications: clock plates and nuts, clock and watch backs, clock gears and wheels, channel plates.

Test specimen: sheet and strip - 1mm thickness.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 55
Hardness, Rockwell 30T 54
Tensile Strength, Ultimate 370 MPa
Tensile Strength, Yield 275 MPa
@Strain 0.5 %
Elongation at Break 35 %In 50 mm
Modulus of Elasticity 97.0 GPa
Poissons Ratio 0.311
Machinability 100 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 37.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000660 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.5 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 115 W/m-K
@Temperature 20.0 °C
Melting Point 885 - 905 °C
Solidus 885 °C
Liquidus 905 °C
Annealing Point 800 - 1100 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 425 - 600 °C
Hot-Working Temperature 700 - 800 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 59 - 64.5 %
Iron, Fe <= 0.10 %
Lead, Pb 2.0 - 3.0 %
Other, total <= 0.50 %
Zinc, Zn 34.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Extra-high-leaded brass, UNS C35600
Extra-high-leaded brass, UNS C35600, OSO35 sheet/strip
Copper, UNS C27000 (Yellow brass), OSO70 Temper flat products
High-leaded brass tube, UNS C33200
Forging Brass, UNS C37700

MC35600b3 / 11235

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.