MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Goodfellow Nickel 70/Copper 30 Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 100 - 260
Tensile Strength at Break 480 - 1200 MPa
Elongation at Break <= 50 %
Tensile Modulus 160 - 180 GPa
Izod Impact, Unnotched 0.900 - 1.60 J/cmNotch Status Unknown
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000480 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.6 - 14.0 µm/m-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 26.0 W/m-K
Melting Point 1300 - 1350 °C
Solidus 1300 °C
Liquidus 1350 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 30 %
Nickel, Ni 70 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MetalTek MTEK 70-30 UNS C96400 Nickel-Copper Alloy
MetalTek MTEK A Cast UNS N04020 Nickel-Copper Alloy
MetalTek MTEK B Cast UNS N24030 Nickel-Copper Alloy
Beryllium Copper, UNS C17200, TB00 Temper Strip
Special Metals MONEL® 404 Copper-Nickel Alloy

NGOODF185 / 16255

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.