MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Arkema Pebax® 3533 SP 01 Polyether Block Amide (PEBA)
Categories: Polymer; Thermoplastic; Polyether Block Amide (PEBA)

Material Notes: Polyether block amide PEBAX® 3533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ISO 1183
 1.00 g/cc0.0361 lb/in³Cond.; ISO 1183
 0.830 g/cc
@Temperature 220 °C
0.0300 lb/in³
@Temperature 428 °F
Melt
Water Absorption 1.2 %1.2 %Dry; Sim. to ISO 62
Moisture Absorption 0.400 %0.400 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/inDry; ISO 294-4, 2577
 0.0080 cm/cm0.0080 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 82
@Time 3.00 sec
82
@Time 0.000833 hour
Dry; ISO 7619-1
Hardness, Shore D 25
@Time 15.0 sec
25
@Time 0.00417 hour
Dry; ISO 7619-1
Tensile Strength at Break 39.0 MPa5660 psiDry; ISO 527-1/-2
Tensile Stress at Strain 2.00 MPa
@Strain 10 %
290 psi
@Strain 10 %
Dry; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
 >= 50 %>= 50 %Cond.; ISO 527-1/-2
 >= 300 %>= 300 %Dry; ISO 527-1/-2
Tensile Modulus 0.0180 GPa2.61 ksiCond.; ISO 527-1/-2
 0.0190 GPa2.76 ksiDry; ISO 527-1/-2
50% Modulus  4.00 MPa
@Strain 50 %
4.00 MPa
@Strain 50 %
Dry; ISO 527-1/-2
 4.00 MPa
@Strain 50 %
4.00 MPa
@Strain 50 %
Cond.; ISO 527-1/-2
100% Modulus 6.00 MPa
@Strain 100 %
870 psi
@Strain 100 %
Dry; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Cond.; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Cond.; ISO 179/1eU
Charpy Impact, Notched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Cond.; ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Cond.; ISO 179/1eA
Tear Strength 50.0 kN/m285 pliDry; ISO 34-1
Abrasion 6464mm³; Dry; ISO 4649
Compression Set 22 %
@Temperature 23.0 °C,
Time 86400 sec
22 %
@Temperature 73.4 °F,
Time 24.0 hour
Dry; ISO 815
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.20e+12 ohm-cm3.20e+12 ohm-cmDry; IEC 60093
Surface Resistance 3.00e+12 ohm3.00e+12 ohmCond.; IEC 60093
Dielectric Constant  6.0
@Frequency 1e+6 Hz
6.0
@Frequency 1e+6 Hz
Dry; IEC 60250
 6.0
@Frequency 100 Hz
6.0
@Frequency 100 Hz
Dry; IEC 60250
Dielectric Strength 33.5 kV/mm851 kV/inDry; IEC 60243-1
Dissipation Factor  0.031
@Frequency 100 Hz
0.031
@Frequency 100 Hz
Dry; IEC 60250
 0.0434
@Frequency 1e+6 Hz
0.0434
@Frequency 1e+6 Hz
Dry; IEC 60250
Comparative Tracking Index 600 V600 VCond.; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 210 µm/m-°C117 µin/in-°FDry; ISO 11359-1/-2
Specific Heat Capacity 2.80 J/g-°C0.669 BTU/lb-°FMelt
Thermal Conductivity 0.180 W/m-K
@Temperature 220 °C
1.25 BTU-in/hr-ft²-°F
@Temperature 428 °F
Melt
Melting Point 144 °C291 °F10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 46.0 °C115 °FDry; ISO 75-1/-2
Vicat Softening Point 77.0 °C171 °F50°C/h 50N; Dry; ISO 306
Glass Transition Temp, Tg -65.0 °C-85.0 °F10°C/min; Dry; ISO 11357-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 °C428 °FInjection Molding; ISO 294
Mold Temperature 30.0 °C86.0 °FInjection Molding; ISO 10724
Injection Velocity 200 mm/sec7.87 in/secInjection Molding; ISO 294
Hold Pressure 30.0 MPa4350 psiInjection Molding; ISO 294
 
Descriptive Properties
Antiblocking agentYes
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
LubricantsYes
Moisture SensitiveYes
Processing MethodsCasting
 Film Extrusion
 Injection Molding
 Other Extrusion
 Profile Extrusion
 Thermoforming
 Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Pebax® 3533 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® 2533 SA 01 Polyether Block Amide (PEBA)
Arkema Pebax® 5533 SP 01 Polyether Block Amide (PEBA)
Arkema Pebax® 2533 SD 02 Polyether Block Amide (PEBA)
Arkema Pebax® 7233 SA 01 MED Polyether Block Amide (PEBA)

PARKG712 / 142507

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.