Product Description: Medium viscosity grade for short cycle times. Chemical abbreviation according to ISO 1043-1: PBT Molding compound ISO 7792-PBT, MGHR, 10-030 Polybutylenterephthalat, nucleated grade with high molecular weight. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Additive: Mold Release Forms: Pellets Processing Method: Injection Molding Information provided by Celanese |