MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Saint-Gobain Norton® OmniFlex™ Fluoroelastomer High Performance Seal Material (Milky White)  (discontinued **)
Categories: Polymer

Material Notes: OmniFlex™ is a fluoroelastomer material with performance equivalent to perfluoroelastomer materials in chemical resistance and inertness yet with a softer durometer and improved compression set. OmniFlex™ has outstanding temperature performance of -70°F (-57°C) which outperforms perfluoroelastomer materials.

SOLVENT COMPATIBILITY: Toluene, Gasoline, Methyl Alcohol, Acetone, Methyl Tertiary Butyl Ether. CHEMICAL COMPATIBILITY: Hydrochloric Acid, Sulfuric Acid, Nitric Acid, Sodium Hydroxide, Butylamine. Typical market applications include Aerospace, Analytical Instrumentation, Petrochemical, Pumps and Valves, Robotics, Automotive and Industrial Finishing, Adhesive Dispensing, Semiconductor Wafer Processing.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040
Tensile Strength, Yield 5.74 MPa833 psi
Elongation at Break 350 %350 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 218 °C425 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
 
Descriptive Properties
ColorMilky White

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Dynaflex™ G7970-1001-00 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE)
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer
ExxonMobil Santoprene® 8191-55B100 Thermoplastic Elastomer
ExxonMobil Santoprene® 8271-75 Thermoplastic Elastomer

PSTGQZ207 / 68721

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.