MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lanxess Zinkoxyd aktiv® Zinc Oxide
Categories: Ceramic; Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes:

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.68 g/cc0.205 lb/in³
Volatiles 0.40 %
@Temperature 110 °C
0.40 %
@Temperature 230 °F
Loss On Ignition <= 4.0 %<= 4.0 %
Specific Surface Area 45 m²/g45 m²/g
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month18.0 Month
 
Component Elements PropertiesMetricEnglishComments
Cadmium, Cd 0.00020 %0.00020 %2 ppm
Lead, Pb 0.00030 %0.00030 %3 ppm
 
Descriptive Properties
Content>93%Zinc oxide
Specifications<0.2%Sieve residue (0.063 mm), DIN ISO 787/18

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NanoScale NanoActive® Zinc Oxide
Zinc Oxide, ZnO, Cubic
Zinc Oxide, ZnO, (Zincite)
Wacker Silfoam® SC 369 Silicone Antifoam Compound
Mateck Zinc Oxide, ZnO

PLANY9183 / 209574

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.