MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess Addocat® 1656 PU Catalyst/Activator
Categories: Other Engineering Material; Catalyst/Initiator

Material Notes: Catalyst for the manufacture of polyurethane (PU) or polyisocyanurate (PIR) rigid foams, especially for continuous production of slabstock foams.

Function: Addocat 1656 is a balanced catalyst mainly used for the production of polyurethane (PU) or polyisocyanurate (PIR) rigid slabstock foams. Addocat 1656 is especially used for the continuous production of rigid slabstock foams.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
Water Absorption <= 0.20 %<= 0.20 %
Viscosity 200 - 260 cP200 - 260 cP
 
Thermal PropertiesMetricEnglishComments
Pour Point -20.6 °C-5.00 °F
Flash Point 71.0 °C160 °FDIN EN 22719
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
Appearancecolorless to slightly yellow liquid
Hydroxyl value84-86 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Baybond® PU 406 Polyurethane
Ensinger Hydex™ 301 Rigid Polyurethane (PU)
Ensinger Hydex™ 202 Rigid Polyurethane (PU)
Covestro Baybond® PU 330 Polyester Urethane Polymer
Covestro Baybond® PU 130 Polyurethane Resin

PLANY8188 / 208581

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.