MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LG Chemical PB1752 PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: General Description: PB1752, homopolymer made from micro-suspension seeded polymerization, is a low-viscosity PVC resin with a pseudo-plastic flow property in processing range. It can be used for skin layer for flooring, tarpaulin made by knife coating and rotary screen coating. Products made from PB1752 are excellent in transparency, matting and physical properties.

Main Applications: Tarpaulin, Rotational molding, Skin layer for flooring

CAS No: 9002-86-2

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.406 g/cc1.406 g/cc
Bulk Density 0.300 - 0.400 g/cc0.0108 - 0.0145 lb/in³ASTM D1895
Volatiles <= 0.30 %
@Temperature 110 °C,
Time 3600 sec
<= 0.30 %
@Temperature 230 °F,
Time 1.00 hour
ASTM D3030-90
Brookfield Viscosity 1000 - 5000 cP1000 - 5000 cPDOP 60phr; ASTM D1824
Viscosity Measurement >= 3.0>= 3.0[g/sec], DOP 60phr, Severs; ASTM D1823
Molecular Weight 60000 - 150000 g/mol60000 - 150000 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 302 °C576 °F
Ignition Temperature 435 °C815 °FAutoignition
 
Descriptive Properties
Degree of Polymerization1600-180030°C, JIS K 6720-2
K-Value76DIN53726 / ISO1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLAY719 / 148729

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.