MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Acetron® POM-H Natural and Black Homopolymer Acetal, Unfilled, Extruded (ASTM Product Data Sheet)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: PLEASE NOTE, BELOW COMPLIANCE INFO IS FOR NATURAL ONLY

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Key Words: POM, Polyoxymethylene; Polyformaldehyde; Polyacetal
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccASTM D792
Water Absorption 0.20 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 0.90 %Immersion; ASTM D570(2)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 89ASTM D785
Hardness, Rockwell R 122ASTM D785
Hardness, Shore D 86ASTM D2240
Tensile Strength 11000 psiASTM D638
Tensile Strength at 65°C (150°F) 7200 psiASTM D638
Elongation at Break 30 %ASTM D638
Tensile Modulus 450 ksiASTM D638
Flexural Strength 13000 psiASTM D790
Flexural Modulus 450 ksiASTM D790
Compressive Strength 15000 psi10% Def.; ASTM D695
Compressive Modulus 300000 psiASTM D695
Shear Strength 9000 psiASTM D732
Izod Impact, Notched 1.00 ft-lb/inASTM D256 Type A
Coefficient of Friction, Dynamic 0.25Dry vs. Steel; QTM55007
K (wear) Factor 200 x 10-10 in³-min/ft-lb-hrQTM 55010
Limiting Pressure Velocity 2700 psi-ft/min4:1 safety factor; QTM 55007
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.00e+13 ohmEOS/ESD S11.11
Dielectric Constant 3.7
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 450 V/milShort Term; ASTM D149
Dissipation Factor 0.0050
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 47.0 µin/in-°F
@Temperature -40.0 - 149 °C
ASTM E831
Thermal Conductivity 2.50 BTU-in/hr-ft²-°FASTM F433
Melting Point 347 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 180 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 250 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
Estimated Rating
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
Canada AG YesNATURAL ONLY
FDA YesNATURAL ONLY
NSF YesNATURAL ONLY
USDA YesNATURAL ONLY
USP Class VI No
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Unacceptable
Acids, Weak Limited
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Limited
Conductive / Static Dissipative No
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Descriptive Properties
Machinability11-10, 1=Easier to Machine

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Delrin Delrin® 150 NC010 POM
Mitsubishi Chemical Advanced Materials Ketron™ 1000 PEEK, Extruded Unfilled Polyetherether Ketone
Celanese Celanex® 2300 GV1/50 PBT, 50% Glass Reinforced
Asahi Kasei TENAC™-C 3510 Copolymer Acetal (POM), High Viscosity
Mitsubishi Chemical Advanced Materials Duratron™ CU60 PBI Polybenzimidazole, unfilled, compression molded

P1SM03 / 20074

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.