MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Beijing Evergrow Resources PTFE Adhesive Tape
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: PTFE adhesive tape is manufactured by PTFE high strength suspension resin. The skived PTFE tape is one side etched, and then coated with adhesive back and chippd to different sizes. It is anticorrosive, insulative and does not age. PTFE Adhesive Tape is widely used in the fields that PVC does not apply to.

Applications: Covers for high performance cables and wires; also covers for cables and wires in high qualified places like hotels, big marketplaces, entertainment places and gymnasiums, etc; covers for cables and wires in open country; sealing for mechanical packers.

Information provided by Beijing Evergrow Resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 25.0 MPa
Elongation at Break 125 %
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength >= 10.0 kV/mm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °C
Minimum Service Temperature, Air -50.0 °C
 
Descriptive Properties
Adhesive Bond Strength (N/25mm)6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.001" thick)
DuPont™ Kapton® 100HN Polyimide Film, 25 Micron Thickness
CEN® Electronic Material CV Polyimide Film, 1 Mil Thickness
3M 5498 PTFE Film Tape
Saint-Gobain Furon®, Kapton® K275 Tape

PBEIJ039 / 90108

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.