MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Geon® Performance Solutions Vinyl Wire & Cable WEAS81L PVC, Flexible  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade; PVC, Wire and Cable Grade

Material Notes: Geon© WEAS81L is a Vinyl Foam Concentrate for Wire and Cable Extrusion. This product is an exothermic type blowing agent intended to be used with a wide range of Wire and Cable Vinyl formulations to provide a degree of foaming under normal conditions of between 10% and 17%. Values of around 10% are recommended to maintain physical properties.

The percentage blow can be reduced by either cutting back on the level of addition or by reducing the air space between the extruder head and the water-cooling trough. The cell structure achieved should be small and just visible under normal viewing, and should be evenly distributed through the extrudate.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 60.0 °C140 °FUL Temperature Rating
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 170 °C>= 338 °FActivation Temperature
 
Descriptive Properties
Addition Percentage Recommended2
FeaturesFoamable
FormsPellets
Processing MethodExtrusion Coating
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesWire & Cable Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PH1PN8996 / 102832

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.