MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Mortars Coastal 90AS Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Crystalline Silica. Material grade: dry, heat setting. Recommended use: Firebrick. Thermal Ceramics refractory mortars were developed to match Thermal Ceramics dense and insulating firebricks in various thermal, chemical, and physical service conditions. Available in wet and dry grades, mortars will provide the convenience you want with the performance you need for practically every high temperature refractory application. Coastal 90™ and Coastal 90 AS™ are a wet and dry version of extra high alumina mortar. They are ideal for 90% alumina brick constructions.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Al2O3 88 %88 %
CaO+MgO 0.10 %0.10 %
Fe2O3 0.20 %0.20 %
K2O+Na2O 2.2 %2.2 %
SiO2 9.0 %9.0 %
TiO2 0.10 %0.10 %
 
Descriptive Properties
Classification Temperature (°C)1816in normal oxidizing conditions
Water Addition23% trowel. 45% dip.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6184 / 202968

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.