MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dow DMDA-8920 NT 7 High Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: DOW DMDA-8920 NT 7 is produced using UNIPOL™ process technology. It is intended for use in a broad range of injection molding applications such as housewares, toys, food containers and pails.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.954 g/cc0.0345 lb/in³ASTM D792
ESCR 100% Igepal® 3.0 hour
@Temperature 50.0 °C
3.0 hour
@Temperature 122 °F
F50; Molded and tested in accordance with ASTM D4976; ASTM D1693
Melt Index of Compound 20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
20 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5757Molded and tested in accordance with ASTM D4976; ASTM D2240
Tensile Strength at Break 13.8 MPa2000 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Tensile Strength, Yield 28.3 MPa4100 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Break 250 %250 %Molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Yield 7.0 %7.0 %Molded and tested in accordance with ASTM D4976; ASTM D638
Flexural Modulus 1.15 GPa
@Strain 2 %
167 ksi
@Strain 2 %
Secant; Molded and tested per ASTM D4976; ASTM D790 B
Tensile Impact Strength 42.0 kJ/m²20.0 ft-lb/in²Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °FDow Method (DSC)
Crystallization Temperature 117 °C243 °FDow Method (DSC)
Deflection Temperature at 0.46 MPa (66 psi) 72.8 °C163 °FMolded and tested in accordance with ASTM D4976; ASTM D648
Vicat Softening Point 127 °C261 °FASTM D1525
Brittleness Temperature <= -76.1 °C<= -105 °FMolded and tested in accordance with ASTM D4976; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUTENE-H ME9180 HDPE
Dow DMDA-8007 NT 7 High Density Polyethylene Resin
Dow DMDA-8907 NT 7 High Density Polyethylene Resin
Chevron Phillips Marlex® 9018 HDPE Injection Molding Resin
Chevron Phillips Marlex® 9035 High Density Polyethylene, Injection Molding

PDOW1263 / 30481

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.