MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

AlphaGary Smokeguard™ FP 108 High Performance Fluoropolymer
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Smokeguard™ FP is a high performance fluoropolymer compound with excellent flame and smoke properties intended for difficult constructions and test requirements
Low smoke, low acid gas fluoropolymer based compound. Applications include Plenum and Limited Combustion Data Cable

Alphagary is part of Orbia.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.92
@Frequency 1e+8 Hz
2.92
@Frequency 1e+8 Hz
Dissipation Factor 0.012
@Frequency 1e+8 Hz
0.012
@Frequency 1e+8 Hz
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 100 %100 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® B 6550 LN PBT
BASF Ultradur® B 6550 L PBT
Arkema Kynar Flex® 3030-15 PVDF
3M Dyneon™ PVDF 11008/0003 Polyvinylidene Fluoride
3M Dyneon™ FEP 6322Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules

PGARY9831 / 140617

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.