MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Escorene® LD-332 EVA Packaging Film Resin, High Clarity  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: Data provided by the manufacturer, Exxon Chemical.

A 1% vinyl acetate copolymer packaging film resin. Film made from LD-332 offers improved impact strength and heat sealability compared to homopolymer clarity film resins. LD-332 can be drawn down to less than 1.0 mil in the blown film process.

Applications: Food packaging (bread bags, baked goods, light duty produce bags, etc.); Frozen food packaging; Profile extrusion; Rack and counter bags where good heat sealability and clarity are required. Data for film properties below based on 1.25 mil film.

Key Words: Ethylene Vinyl Acetate; Exxon Chemical Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.927 g/ccExxon Method
Thickness 1.25 mil
Melt Flow 2.0 g/10 minExxon Method
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 10.0 MPaASTM D882
Film Tensile Strength at Yield, TD 11.0 MPaASTM D882
Film Elongation at Break, MD 225 %ASTM D882
Film Elongation at Break, TD 600 %ASTM D882
Secant Modulus, MD 0.250 GPaASTM D882
Secant Modulus, TD 0.330 GPaASTM D882
Elmendorf Tear Strength MD 600 gASTM D1922
Elmendorf Tear Strength TD 150 gASTM D1922
Elmendorf Tear Strength, MD 480 g/milASTM D1922
Elmendorf Tear Strength, TD 120 g/milASTM D1922
Dart Drop 64.0 g/milF50; ASTM D1709
Dart Drop Test 80.0 gF50; ASTM D-1709
Film Tensile Strength at Break, MD 31.0 MPaASTM D882
Film Tensile Strength at Break, TD 22.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 110 °CExxon Method
 
Optical PropertiesOriginal ValueComments
Haze 3.7 %ASTM D1003
Gloss 77 %45°, ASTM D-2457
Transmission, Visible 90 %clear; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEXCDG / 37856

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.