MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nylene® PX1719 Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Dry as molded. Extrusion grade. Nylene PX1719HS is a heat stabilized, high impact, nylon 6 extrusion grade resin with a low flexural modulus. PX1719HS is ideally suited for extrusion of tubing and profiles requiring outstanding toughness and flexibility. Because of its excellent flow characteristics, it may also be used for injection molding parts requiring a high Izod impact value. Optimum processing conditions should provide a melt temperature of 520 - 540ºF at the die or nozzle.

ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.

Key Words: Polyamide 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 62.0 MPaASTM D638
Elongation at Break 250 %ASTM D638
Flexural Modulus 0.660 GPaASTM D790
Izod Impact, Notched 8.30 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 141 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 275 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ashley Polymers Ashlene® 527 Nylon 66
Adell BD-10 Nylon 6, Ultra High Impact
Kolon KOPA® KN173HI4 High Impact Nylon 6
Trinseo Magnum™ 1040 ABS, Very High impact
Kolon KOPA® KN173HI3R High Impact Nylon 6

PN6C59 / 54243

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.