MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company PermaStat PLUS® 2500 A Polycarbonate/ABS Alloy (PC/ABS); Permanently Static Dissipative - ESD Protection
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate (PC)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D 792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0060 - 0.0080 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 46.2 MPa6700 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Tensile Modulus 1.79 GPa260 ksiASTM D 638
Flexural Strength 75.8 MPa11000 psiASTM D 790
Flexural Modulus 2.07 GPa300 ksiASTM D 790
Izod Impact, Notched 11.7 J/cm
@Thickness 3.20 mm
22.0 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
NB
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+7 - 9.90e+8 ohm-cm1.00e+7 - 9.90e+8 ohm-cmASTM D 257
Surface Resistance 1.00e+7 - 9.90e+8 ohm1.00e+7 - 9.90e+8 ohmESD STM11.11
Surface Resistivity per Square 1.00e+8 - 9.90e+9 ohm1.00e+8 - 9.90e+9 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secFTMS101C; 4046.1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 216 - 249 °C420 - 480 °F
Mold Temperature 51.7 - 79.4 °C125 - 175 °F
Drying Temperature 93.3 °C
@Time 14400 sec
200 °F
@Time 4.00 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman SCHULAMID® 66 PTFE20 HS 20% PTFE Lubricated, Heat Stabilized Nylon 6/6
RTP Company PermaStat PLUS® 2501 A Polycarbonate/ABS Alloy (PC/ABS); ESD Protection - Permanently Static Dissipative - Glass Fiber - Preliminary
RTP Company ESD 4485 High Temperature Nylon (HTN); Carbon Fiber - ESD Protection - Electrically Conductive
RTP Company EMI 2562 UV BLACK Polycarbonate/ABS Alloy (PC/ABS); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive - UV Stabilized
RTP Company EMI 2561 FR UV Polycarbonate/ABS Alloy (PC/ABS); Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding - Flame Retardant - UV Stabilized

PQZRA31866 / 206026

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.