MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Permabond 935 Cyanoacrylate
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: The PERMABOND 930 series is a family of low odor, non-fogging, non-frosting cyanoacrylates. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesives on hot and humid days, is eliminated. The elimination of fogging improves the production rate of acceptable parts as well as their appearance.

Features & Benefits:

  • Low odor
  • Eliminates whiting (frosting and fogging) of parts
  • Excellent adhesion to a wide variety of surfaces
  • Good flexibility and impact resistance

Typical Applications:

  • Black or dark plastic and metal surface facia
  • Where ventilation is limited or difficult
  • Visible bondlines on appliances or cabinets
  • Nameplates

Soluble in Nitroethane, Methyl Ethyl Ketone, Acetone.

Information provided by Permabond.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 400 - 600 cP
@Temperature 20.0 °C
400 - 600 cP
@Temperature 68.0 °F
Uncured
Storage Temperature 2.00 - 7.00 °C35.6 - 44.6 °F
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 0.690 MPa100 psiABS, Substrate Failure, Shear; ASTM D1002
 1.38 MPa200 psiPolystyrene, Substrate Failure, Shear; ASTM D1002
 1.72 MPa249 psiAcrylic, Substrate Failure, Shear; ASTM D1002
 2.10 MPa305 psiEPDM, Substrate Failure, Shear; ASTM D1002
 4.10 MPa595 psiPVC, Substrate Failure, Shear; ASTM D1002
 6.90 MPa1000 psiAluminum, Shear; ASTM D1002
 13.8 MPa2000 psiGrit Blasted Steel, Shear; ASTM D1002
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 75.0 °C167 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Flash Point >= 110 °C>= 230 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 0.0833 - 0.167 min0.00139 - 0.00278 hourSteel, set time
 0.0833 - 0.167 min0.00139 - 0.00278 hourBuna N Rubber, set time
 0.167 - 0.333 min0.00278 - 0.00556 hourPhenolic, set time
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
full strength
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceColorlessUncured
Maximum Gap Fill (mm)0.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 316 Cast Stainless Steel, SUS316 Hot Formed
Versalis KOBLEND PCA PD 935 G2 PC+ABS, 10% Glass Fiber
Unipetrol PP MONSTEN® MT 935 Polypropylene Random Copolymer
Overview of materials for Low Carbon Steel
Chevron Phillips Marlex® HMN TR-935/935G Polyethylene; MDPE

PPERMA882 / 162763

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.