MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Soarus SoarnoL® D2908 Ethylene Vinyl Alcohol Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Alcohol (EVOH)

Material Notes: Ethylene content 29 mol%. Volatile matter 0.3%.

The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a thin gas barrier layer without loss of shelf life.

Soarnol D2908 with intermediate melt flow index is one of the standard grade of Soarnol, its ethylene content is 29 mol%. Since Soarnol D2908 has a good gas barrier at low humidity, this resin is suited for coextruded film and coextrusion coating. This resin can also be used in coextruded sheet, coextruded blow-molded containers and coextruded pipe.

Processing: Extruder:40 m screw type, L/D=28;Screw:Full-flighted, constant pitch type, CR=4.0;Screen pack:80/120/50 mesh;Die:Manifold type, die width=450 mm, lip distance=0.2 mm.

Information provided by Soarus, LLC. In the United States SOARNOL is produced by Noltex, L.L.C., an affiliate of Nippon Gohsei.

Key Words: EVOH
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/cc
Moisture Vapor Transmission 1.11 - 2.10 cc-mm/m²-24hr-atm40°C- 90% RH; based on 30 µm layer
Oxygen Transmission 0.00800 cc-mm/m²-24hr-atm20°C- 65% RH; based on 20 µm layer
Viscosity 500000 cP
@Shear Rate 250 1/s,
Temperature 230 °C
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 210 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 188 °CDSC, both heating and cooling speeds of 20°C/min
Crystallization Temperature 163 °CDSC, both heating and cooling speeds of 20°C/min
Glass Transition Temp, Tg 62.0 °CDSC, both heating and cooling speeds of 20°C/min
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.525Quenched
 1.534Annealed at 140°C, 30 min
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 200 - 220 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Soarus SoarnoL® AT4403 Ethylene Vinyl Alcohol Copolymer
Soarus SoarnoL® DC3203F Ethylene Vinyl Alcohol Copolymer
Soarus SoarnoL® DT2903 Ethylene Vinyl Alcohol Copolymer
Soarus SoarnoL® A4412 Ethylene Vinyl Alcohol Copolymer
Soarus SoarnoL® BS3803 Ethylene Vinyl Alcohol Copolymer

PSOAR01 / 67861

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.