MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

CHT ACC34 Silicone Diluent
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Characterization: ACC34 thinner is a low viscosity silicone diluent that can be employed as viscosity modifier for many 1- Part RTV sealants, and conformal coatings. It is available as the standard version and an optional UV fluorescing version (ACC34UV). The ACC34UV version is especially recommended for higher dilution ratios of ACC15, 16 and 17 to maintain a high level of UV fluorescence ACC34 thinner is volatile. It will be lost slowly at room temperature from a thin section of cured silicone rubber or coating, but is readily removed at temperatures from 80°C to 150°C. In the case of 1- Part RTV's this heating cycle is best carried out after 8 hours of curing, for ACC16, the heating cycle can begin after 90 minutes of curing and for ACC17 the heating cycle can begin after 16 to 40 minutes of curing, depending on the dilution ratio. ACC34 thinner has not been classified as a Volatile Organic Compound (VOC) and no legislation to this effect is expected. It is a cosmetically approved ingredient and is a much safer choice than conventional organic solvents for many reasons, a few of which are:
  • wide liquid temperature range
  • odourless
  • not regarded as an environmental hazard
  • extremely low toxicity (oral LD50 = 35,000 mg/kg)
  • compatible with virtually all silicones
  • very low surface tension (<18 N/m) which enhances spreading of films.
  • good rate of evaporation considering its high boiling point (205°C), due to unusually low heat of vaporisation.
  • high Flash Point (not classified as flammable)

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 0.00 %0.00 %
Viscosity Measure 5.0 cSt5.0 cSt
Surface Tension 18 dynes/cm18 dynes/cm
 
Thermal PropertiesMetricEnglishComments
Melting Point <= -50.0 °C<= -58.0 °F
Boiling Point 205 °C401 °F
Flash Point 77.0 °C171 °F
Ignition Temperature >= 400 °C>= 752 °FAuto
 
Component Elements PropertiesMetricEnglishComments
Nitrogen, N 1.5 %1.5 %
 
Descriptive Properties
ColorClear
Evaporation rate12(Butyl acetate =100; White spirit = 14), BS ISO 2781
Latent heat of vaporization113 KJ/kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL192 / 314675

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.