MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® A3EG3 BK00564 15% Glass Filled PA66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: Ultramid A3EG3 BK00564 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccISO 1183
Water Absorption 7.0 %ISO 62
Moisture Absorption at Equilibrium 2.2 %23°C/50% R.H.; ISO 62
Viscosity Number 149 cm³/g
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 122 MPa5mm/min; ISO 527
Elongation at Break 2.5 %5mm/min; ISO 527
Izod Impact, Notched (ISO) 5.50 kJ/m²ISO Test
Charpy Impact, Notched 0.550 J/cm²ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 33.0 µm/m-°CISO 11359
CTE, linear, Transverse to Flow 75.0 µm/m-°CISO 11359
Melting Point 260 °C10 K/min
Deflection Temperature at 1.8 MPa (264 psi) 246 °CISO 75
Flammability, UL94 HB
@Thickness 1.66 mm
 HB
@Thickness 0.810 mm
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
ColorBK00564
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry)
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Dry)
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Dry)
BASF Ultramid® 7423-2 NF3001 13% Glass Filled PA66 (Dry)

PBASF9219 / 84983

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.