MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

CHT SilSo CONNECT 21000 Silicone elastomer
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: This is a two component silicone elastomer which crosslinks through polyaddition reaction. Particularly well suited for LSR applications and when processing with injection molding equipment.

Key Features

  • Electrically conductive
  • Non-corrosive
  • Heat curing
  • Low linear shrinkage
Application: Smart textiles. Pressure sensors, RFI gaskets and shielding - application by coating or liquid injection molding

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³A
 1.10 g/cc0.0397 lb/in³B
Brookfield Viscosity 71000 cP71000 cPA
 75000 cP75000 cPB
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3535DIN 53 505
Tensile Strength 1.90 MPa276 psiISO 37
Elongation at Break 240 %240 %ISO 37
Tear Strength 5.61 kN/m32.0 pliBS ISO 34-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1000 ohm-cm>= 1000 ohm-cmASTM D-257
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.350 W/m-K2.43 BTU-in/hr-ft²-°F
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min
@Temperature 100 - 130 °C
1.00 hour
@Temperature 212 - 266 °F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorBlackA
 BlackB
 BlackCured Product
Cure typeAddition
RheologyViscous liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL067 / 314550

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.