MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Syensqo (Solvay Specialty Polymers) Hylar® 5000 HG PVDF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Hylar® 5000 HG is a crystalline high molecular weight powder form of polyvinylidene fluoride (PVDF)specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically strong and tough films that have a broad useful temperature range. These films are highly resistant to most environmental conditions including gamma radiation and are essentially transparent to ultraviolet radiation. The weathering characteristics of Hylar® 5000 HG coatings lead to excellent performance for the long term.

Hylar® 5000 is available only via a licensing program that specifies the composition of Hylar® 5000 HG coatings. A properly formulated finish contains sufficient pigment to make the film totally opaque to ultraviolet radiation at the nominal one mil (0.001 inch) film thickness suggested.

SAFETY
Hylar® 5000 HG is stable at temperatures up to 600°F (316°C). When it is subjected to temperatures above 600°F (316°C) for extended periods of time, hydrogen fluoride (HF) begins to evolve, and at temperatures above 700°F (371°C) HF evolution becomes rapid. Hylar® 5000 HG exhibits excellent flame resistance; however, in case of fire, HF and traces of potentially toxic fluorocarbons can be formed. HF is corrosive, causes burns on contact, and has an American Conference Governmental Industrial Hygienists (ACGIH) Threshold Limit Value (TLV-TWA) of 3 ppm (2.5 mg/m³) (1984).

Thermal decomposition of Hylar® 5000 HG to HF can also occur in a bake oven in the event that temperatures are not controlled properly. In the event of fire, use NIOSH approved self-contained breathing apparatus and skin protection to protect against volatile decomposition products. Hylar® 5000 HG can be disposed of in an approved land fill, but should not be incinerated unless permitted by applicable law and provision is made for absorption of HF.

Applications: Coating Applications; Film

Features: Clean/High Purity; Crystalline; Good Strength; Good Toughness; Good Weather Resistance; High Gloss; High Molecular Weight; Low Odor; Radiation (Gamma) Resistant; UV Resistant

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 - 1.77 g/cc0.0632 - 0.0639 lb/in³ASTM D792
Water Absorption at Saturation 0.040 %0.040 %ASTM D570
Viscosity 1750 - 2050 cP1750 - 2050 cPMelt; ASTM D3835
 
Thermal PropertiesMetricEnglishComments
Melting Point 164 - 167 °C327 - 333 °F
 
Optical PropertiesMetricEnglishComments
Gloss >= 40 %>= 40 %ASTM D523
 
Descriptive Properties
AvailabilityEurope
 North America
ColorWhite
FormsPowder
ProcessingCoating

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4256 / 280056

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.