MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ Resin 2210 Polyetherimide (PEI) (Asia)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.

Features: High Stiffness,Hydrolytic Stability,Chemical Resistance,Easy Flow,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,General Purpose,High Heat Resistance,Good dimensional stability,Flame Retardant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
Melt Flow 8.4 g/10 min
@Load 6.60 kg,
Temperature 337 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 114ASTM D785
Tensile Strength at Break 139 MPa5 mm/min; ASTM D638
Elongation at Break 4.0 %5 mm/min; ASTM D638
Tensile Modulus 6890 MPa5 mm/min; ASTM D638
Flexural Strength 227 MPabrk, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 6890 MPa2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 64.0 JASTM D256
 453 J
@Thickness 3.20 mm
reverse notched; ASTM D256
Izod Impact, Unnotched 475 J/mASTM D4812
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 100 - 175 VUL 746A
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness >=1.50 mm
UL 746A
 60 - 120 sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=3.00 mm
UL 746A
 15 - 30 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 21.0 µm/m-°C
@Temperature -20.0 - 150 °C
ISO 11359-2
CTE, linear, Transverse to Flow 49.0 µm/m-°C
@Temperature -20.0 - 150 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 211 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 225 °CRate B/50; ASTM D1525
UL RTI, Electrical 170 °CUL 746B
UL RTI, Mechanical with Impact 170 °CUL 746B
UL RTI, Mechanical without Impact 170 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.380 mm
UL 94
Smoke Density 1.3Flaming, Ds 4 min; ASTM E662
Oxygen Index 50 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 345 - 400 °C
Zone 2 340 - 400 °C
Zone 3 345 - 400 °C
Melt Temperature 350 - 400 °CInjection Molding
Mold Temperature 135 - 165 °C
Drying Temperature 150 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
 24.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82524 / 290471

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.