MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Superior Flux Superior No. 25 Silver Brazing Liquid
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • VOC-Free Flux
  • Excellent choice for jewelry, musical instruments and other applications.
  • Boosts productivity, efficiency, and output for SS409 Tube Welding
Description: Superior No. 25 is a VOC-Free, liquid brazing flux, containing borates and fluorides. It performs well on ferrous and non-ferrous alloys, as well as precious metals. The flux exhibits excellent capillary action, drawing the silver solder into narrow joints. Furthermore, it exerts powerful scavenging action on most metal oxides, removing tarnish, scale, and other impurities yielding strong brazed joints.

Applications: Superior No. 25 is used for brazing in furnaces with poor atmospheres for joining jewelry parts and musical instruments, and for any brazing job that requires a liquid flux. Another application is in Tube Welding where the flux reduces electrical requirements in induction process, removes oxide levels on surface to yield a better, stronger joint.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/cc
pH 7.7
 
Thermal PropertiesOriginal ValueComments
Melting Point -6.00 °CFreezing Point
Boiling Point 106 °C
Maximum Service Temperature, Air 590 - 870 °CActive Range
 
Processing PropertiesOriginal ValueComments
Shelf Life 2.00 Month
 
Descriptive Properties
FormClear liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Indium Corp. Indalloy 215 Silver Solder Alloy
Nickel silver 65-10, UNS C74500, OSO70 Temper flat products
Potters Industries Conduct-O-Fil® AG-SL150-16-TRD Silver-coated Hollow Ceramic Spheres
Silver Aluminum Sulfide, AgAlS2
Silver-Copper Eutectic Alloy (72Ag-28Cu; UNS P07720; AWS BAg-8), Cold Drawn then Annealed at 250°C (480°F)

NSFLUX010 / 185694

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.