MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
ITW Insulcast® RTVS 8128 Silicone Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. RTVS 8128 is a low viscosity Flame Retardant, general purpose, reversion resistant RTV Silicone. With the ability to cure rapidly at elevated temperature, RTVS 8128 combines the virtues of low temperature flexibility, excellent electrical properties, high temperature resistance and easy removal for component replacement or repair. Meets the requirements of UL 94V-0.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccUncured. Part B
 1.38 g/ccUncured. Part A
Viscosity 2000 cPMixed, Part A, Part B; ASTM D1084
 2000 cPPart A; ASTM D1084
 2000 cPPart B; ASTM D1084
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A >= 45ASTM D2240
 <= 55
Tensile Strength 500 psiASTM D412
Elongation at Break 135 %ASTM D412
Tear Strength 18.0 pliDie B; ASTM D624
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.50e+15 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 550 V/milASTM D149
Dissipation Factor 0.0070
@Frequency 1000 Hz
ASTM D150
Comparative Tracking Index >= 600 V
Hot Wire Ignition, HWI 30 - 60 sec
High Amp Arc Ignition, HAI 60 - 120 arcs
 
Thermal PropertiesOriginal ValueComments
CTE, linear 220 µm/m-°C
Thermal Conductivity 0.180 W/m-K
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -55.0 °C
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Cure Time 0.250 hour
@Temperature 120 °C
option
 1.00 hour
@Temperature 90.0 °C
option
 4.00 hour
@Temperature 60.0 °C
option
 24.0 hour
@Temperature 25.0 °C
option
Pot Life 60.0 - 90.0 minPart A, Part B
Gel Time 240 - 360 minuncured. Part A, Part B
Shelf Life 12.0 MonthPart A, Part B
 
Descriptive Properties
ColorBuff (Neutral)part B, uncured
 Dark Graypart A, uncured
Mix Ratio by volume1:1Part A: Part B
Mix Ratio by weight1:1Part A: Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWIN9126 / 239636

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.