MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eastman Aerafin™ 18 Propylene-based olefin polymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: Eastman Aerafin™ 180 polymer is a fully saturated, low molecular weight, propylene-based olefin polymer that is compatible with a range of hydrocarbon tackifying resins and enables spraying the finished adhesive at a broad range of temperatures and operating conditions. Aerafin™ 180 polymer is characterized by consistent quality, low color, excellent thermal stability, and low odor.

Application/Uses:

  • Hot Melt Adhesives
  • Hygiene Construction
  • Nonwovens
Key Attributes:
  • Compatibility with an array of hydrocarbon tackifying resins
  • Excellent thermal stability
  • Good adhesion with excellent peel strength
  • In formulation, enables a robust adhesive system with a broad processing window and sprayability at temperatures as low as 130°C
  • Low color and odor
  • Reliable global supply
  • Requires lower tackifier loading than with most SBC-based formulations

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 18000 cP
@Temperature 190 °C
18000 cP
@Temperature 374 °F
ASTM D3236
 
Mechanical PropertiesMetricEnglishComments
Penetration 2525[dmm], Hardness; ASTM D5
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -38.0 °C-36.4 °FASTM D3418
Ring & Ball Softening Point 125 °C257 °FASTM E 28
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 1.01.0Molten
 
Descriptive Properties
AppearancePellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5123 / 222317

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.