MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Mocom (ALBIS) ALTECH® PA66 ECO 2020/116 GF20 IM Nylon 66, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: Base Polymer: Polyamide 66

Filler/Additive System: 20% glass fibers

Special Features: Impact modified, contains recycled material

Market Segment: Automotive, Building and Construction, various

Application Area: Cooling system, filter systems, transport systems, various

Typical Application: Oil pump parts, housing and automotive trim unpainted, various

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ISO 1183
Maximum Moisture Content 0.150.15
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Time 86400 sec
0.0040 - 0.0060 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cm
@Time 86400 sec
0.0070 - 0.010 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 35 g/10 min
@Load 5.00 kg,
Temperature 275 °C
35 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 110 MPa16000 psiISO 527
Elongation at Break 3.0 %3.0 %ISO 527
Tensile Modulus 6.50 GPa943 ksiISO 527
Flexural Strength 180 MPa26100 psiISO 178
Flexural Modulus 6.00 GPa870 ksiISO 178
Charpy Impact Unnotched  3.00 J/cm²
@Temperature -40.0 °C
14.3 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eU
 3.50 J/cm²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 0.400 J/cm²
@Temperature -40.0 °C
1.90 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 225 °C437 °FISO 75-1/-2
Vicat Softening Point 240 °C464 °FB50; ISO 306
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °FInjection molding
Mold Temperature 80.0 - 120 °C176 - 248 °FInjection molding
Drying Temperature 80.0 °C
@Time 7200 - 43200 sec
176 °F
@Time 2.00 - 12.0 hour
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolyamide 66

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PALBIS8770 / 242829

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.