MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dow FLEXOMER™ DFDA-1137 NT 7 Very Low Density Polyethylene (VLDPE) Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: FLEXOMER™ DFDA-1137 NT 7 is an ethylene copolymer intended for use in molding and extrusion applications where high flexibility is desired. It is especially useful for flexible hose and tube applications as well as for blow molding small squeezable bottles. It has a high molecular weight and a relatively narrow molecular weight distribution and exhibits excellent low temperature toughness and outstanding flex life characteristics. It is also recommended as a blending component to modify and improve the physical properties of high pressure and linear low density polyethylene resins.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccnatural resin; ASTM D792
Environmental Stress Crack Resistance >= 500 hourF0; Compression molded parts prepared according to ASTM D 1928, condition A.; ASTM D1693
Melt Index of Compound 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 94Compression molded parts per ASTM D 1928 Procedure C.; ASTM D676
Tensile Strength at Break 2800 psiCompression molded parts per ASTM D 1928 Procedure C.; ASTM D638
Elongation at Break 900 %Compression molded parts per ASTM D 1928 Procedure C.; ASTM D638
1% Secant Modulus 17000 psiCompression molded parts per ASTM D 1928 Procedure C.; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 244 °FDow Method (DSC)
Vicat Softening Point 187 °FASTM D1525
Brittleness Temperature <= -148 °FCompression molded parts prepared according to ASTM D 1928, procedure A.; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow FLEXOMER™ DFDA-1098 NT Very Low Density Polyethylene (VLDPE) Resin
Dow FLEXOMER™ DFDB-1088 NT Very Low Density Polyethylene (VLDPE) Resin
Dow FLEXOMER™ DFDA-1010 NT 7 Very Low Density Polyethylene (VLDPE) Resin
Dow FLEXOMER™ DFDB-9042 NT Very Low Density Polyethylene (VLDPE) Resin
Dow FLEXOMER™ GRSN-1539 NT 7 Very Low Density Polyethylene (VLDPE) Resin

PDOW1375 / 30593

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.