MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Go Yen Chemical GoyenchemUV-706 Anti-UV Agent for Nylon plastic
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GoyenchemUV-706, a special anti-UV additive for yellowing deterioration and weather-resistance of PA resin series, it can block outdoor sunlight and UV rays, also can effectively provide products with anti-UV properties, not only to enhance the product resistance for sunlight and yellowing, but also can improve added value of the product.

Advantages:

  • Excellent UV resistance, weather resistance.
  • Delay the degradation, aging rate of products, greatly enhance anti-UV properties of products.
  • Suitable with all kinds of engineering plastics, outstanding compatibility, does not affect the processing performance and physical properties of the products.
  • Provide product stability and storage stability.
  • Increase the additive value of products.
  • Well-known nylon manufacturers specified product.
Applications:
  • Polyamide(Nylon) resin series:Nylon, Nylon6, Nylon6,6, PAII, PA46, PA6T
  • Polyacetal rein, polyurethane resin, TPU resin, adhesive, RIM
  • Polypropylene, polyethylene, polystyrene
  • Various indoor and outdoor paint, powder coating
  • Automotive interior, exterior parts product

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 - 1.15 g/cc0.0379 - 0.0415 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 100 °C<= 212 °F
 
Descriptive Properties
AppearanceSolid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN495 / 266803

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.