MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Unitika M1030B PA6, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Nano composite nylon

Information provided by Unitika Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Water Absorption 1.0 %
@Time 86400 sec
1.0 %
@Time 24.0 hour
Moisture Absorption at Equilibrium 2.8 %2.8 %50% RH
Linear Mold Shrinkage, Flow 0.0080 cm/cm
@Thickness 3.20 mm
0.0080 in/in
@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.010 cm/cm
@Thickness 3.20 mm
0.010 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 113113ASTM D785
Tensile Strength at Break 85.0 MPa12300 psiASTM D638
Elongation at Break 20 %20 %ASTM D638
Flexural Strength 133 MPa19300 psiASTM D790
Flexural Modulus 3.70 GPa537 ksiASTM D790
Compressive Strength 85.0 MPa12300 psiASTM D362
Shear Strength 62.0 MPa8990 psiASTM D732
Izod Impact, Notched 0.400 J/cm0.749 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmASTM D257
Dielectric Strength 27.0 kV/mm686 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unitika M1030B PA6, Conditioned
Envalior Akulon® F136-C PA6
Envalior Akulon® F132 PA6
Domo TECHNYL® 1021ST PA6, DRY
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Conditioned)

PUNITIK845 / 177865

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.