MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
KEP Kepital® F20-51 Acetal Copolymer, Black UV & Weather Resistance Grade
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: UV resistance with UV carbon black, medium viscosity grade, good for weather resistance purpose. It has stability on UV light, and so good at out-door use.

Information provided by KEP Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183
Water Absorption 0.20 %ISO 62
Linear Mold Shrinkage, Flow 0.020 cm/cmt = 3 mm
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 62.0 MPa50 mm/min; ISO 527
Elongation at Break 25 %50 mm/min; ISO 527
Elongation at Yield 9.0 %50 mm/min; ISO 527
Flexural Strength 88.0 MPaISO 178
Flexural Modulus 2650 MPaISO 178
Charpy Impact, Notched 7.50 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohmIEC 60093
Dielectric Strength 19.0 kV/mmIEC 60243
 
Thermal PropertiesOriginal ValueComments
CTE, linear 130 µm/m-°CISO 11359
Melting Point 165 °CISO 3146

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
KEP Kepital® F30-51 Acetal Copolymer, Black UV & Weather Resistance Grade
Renishaw 8045 Polyurethane Resin
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin
Mitsubishi Iupital® F30-03 Copolymer Acetal
Overview of materials for Acetal Copolymer, Unreinforced

PKEP9908 / 185584

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.