MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott N-LAF33 Glass
Categories: Ceramic; Glass

Material Notes:

Information Provided by SCHOTT North America, Inc.

Key Words: 786441.436
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.36 g/cc0.158 lb/in³
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 52.252.2
Alkali Class, AR 1.01.0
Stain Resistance Class, FR 2.02.0
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 730730.1/20
Modulus of Elasticity 111 GPa16100 ksi
Poissons Ratio 0.3010.301
Shear Modulus 43.0 GPa6240 ksicalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear  5.60 µm/m-°C
@Temperature -30.0 - 70.0 °C
3.11 µin/in-°F
@Temperature -22.0 - 158 °F
 6.70 µm/m-°C
@Temperature 20.0 - 300 °C
3.72 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.570 J/g-°C0.136 BTU/lb-°F
Thermal Conductivity 0.800 W/m-K5.55 BTU-in/hr-ft²-°F
Transformation Temperature, Tg 600 °C1110 °F
Softening Point 673 °C1240 °FViscosity 107.6 dPa s
Annealing Point 585 °C1090 °FViscosity 1013.0 dPa s
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.78582
@Wavelength 587.6 nm
1.78582
@Wavelength 587.6 nm
nd
 1.79007
@Wavelength 546.1 nm
1.79007
@Wavelength 546.1 nm
ne
Abbe Number 43.843.8ve
 44.0544.05vd
Optical Dispersion 0.0178390.017839nf - nc
 0.0180380.018038nf' - nc'
Transmission, Visible  91 %
@Thickness 10.0 mm,
Wavelength 380 nm
91 %
@Thickness 0.394 in,
Wavelength 380 nm
 96.2 %
@Thickness 10.0 mm,
Wavelength 405 nm
96.2 %
@Thickness 0.394 in,
Wavelength 405 nm
 98.7 %
@Thickness 10.0 mm,
Wavelength 460 nm
98.7 %
@Thickness 0.394 in,
Wavelength 460 nm
 99.7 %
@Thickness 10.0 mm,
Wavelength 580 nm
99.7 %
@Thickness 0.394 in,
Wavelength 580 nm
 99.8 %
@Thickness 10.0 mm,
Wavelength 700 nm
99.8 %
@Thickness 0.394 in,
Wavelength 700 nm
IR Transmittance  46.8 %
@Thickness 10.0 mm,
Wavelength 2500 nm
46.8 %
@Thickness 0.394 in,
Wavelength 2500 nm
 98.8 %
@Thickness 10.0 mm,
Wavelength 1530 nm
98.8 %
@Thickness 0.394 in,
Wavelength 1530 nm
UV Transmittance  1.7 %
@Thickness 10.0 mm,
Wavelength 320 nm
1.7 %
@Thickness 0.394 in,
Wavelength 320 nm
 24.6 %
@Thickness 10.0 mm,
Wavelength 334 nm
24.6 %
@Thickness 0.394 in,
Wavelength 334 nm
 60.1 %
@Thickness 10.0 mm,
Wavelength 350 nm
60.1 %
@Thickness 0.394 in,
Wavelength 350 nm
 85.7 %
@Thickness 10.0 mm,
Wavelength 370 nm
85.7 %
@Thickness 0.394 in,
Wavelength 370 nm
 
Descriptive Properties
B0
Climatic Resistance Test CR1
HG1
K (10-6mm2/N)2.21
Phosphate Resistance PR3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Corning Willow® Flexible Display Glass
American Computer Optics 15in Tempered LCD Glass
Ohara BSM51Y i-Line Optical Glass
Saint-Gobain Spectrosil® 2000 Optical Fused Quartz
Saint-Gobain Spectrosil® 2200 Optical Fused Quartz

CSGS056 / 93390

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.