MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC XENOY™ X5300WX PC+PBT (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/ccASTM D792
Density 1.23 g/cc0.0444 lb/in³ISO 1183
Water Absorption 0.50 %0.50 %23°C/sat; ISO 62
Moisture Absorption 0.150 %0.150 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm
@Thickness 3.20 mm
0.0070 - 0.0090 in/in
@Thickness 0.126 in
SABIC method
Melt Flow  25 g/10 min
@Load 5.00 kg,
Temperature 265 °C
25 g/10 min
@Load 11.0 lb,
Temperature 509 °F
cm³/10 min; ISO 1133
 26 g/10 min
@Load 5.00 kg,
Temperature 266 °C
26 g/10 min
@Load 11.0 lb,
Temperature 511 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 51.0 MPa7400 psi50 mm/min; ISO 527
 51.0 MPa7400 psi50 mm/min; ASTM D638
Tensile Strength, Yield 62.0 MPa8990 psi50 mm/min; ASTM D638
 62.0 MPa8990 psi50 mm/min; ISO 527
Elongation at Break 110 %110 %50 mm/min; ASTM D638
 110 %110 %50 mm/min; ISO 527
Elongation at Yield 5.0 %5.0 %50 mm/min; ASTM D638
 5.0 %5.0 %50 mm/min; ISO 527
Tensile Modulus 2.25 GPa326 ksi1mm/min; ISO 527
 2.55 GPa370 ksi50 mm/min; ASTM D638
Flexural Yield Strength 87.0 MPa12600 psi2 mm/min; ISO 178
 96.0 MPa13900 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.18 GPa316 ksi2 mm/min; ISO 178
 2.48 GPa360 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 7.47 J/cm14.0 ft-lb/inASTM D256
 1.80 J/cm
@Temperature -30.0 °C
3.37 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 50.0 kJ/m²23.8 ft-lb/in²80*10*4; ISO 180/1A
 15.0 kJ/m²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 4.50 J/cm²21.4 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 71.0 J52.4 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 70.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
39.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow  75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 75.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
42.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
@Thickness 3.20 mm
214 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 89.0 °C192 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 87.0 °C
@Thickness 3.20 mm
189 °F
@Thickness 0.126 in
unannealed; ASTM D648
 88.0 °C
@Thickness 6.40 mm
190 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 120 °C248 °FRate B/50; ISO 306
 124 °C255 °FRate B/120; ISO 306
 135 °C275 °FRate B/50; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 255 - 270 °C491 - 518 °FInjection Molding
Zone 1 245 - 265 °C473 - 509 °F
Zone 2 250 - 270 °C482 - 518 °F
Zone 3 255 - 275 °C491 - 527 °F
Melt Temperature 260 - 275 °C500 - 527 °F
Mold Temperature 65.0 - 90.0 °C149 - 194 °F
Drying Temperature 110 °C230 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %0.020 %
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 50 - 80 %50 - 80 %
Vent Depth 0.00130 - 0.00200 cm0.000512 - 0.000787 in
Screw Speed 50 - 80 rpm50 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10866 / 244333

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.