MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Covestro Makrolon® LD sheet Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Light diffusing Makrolon® LD sheet is a polycarbonate product designed with an advanced light diffusion technology that provides excellent light uniformity without sacrificing light transmission. The proprietary diffuser technology eliminates visible hot spots from pinpoint LED lights in typical flat and formed sign applications. LD is available in a range of standard sign colors and can be custom matched to any color. Makrolon LD is easy to form, fabricate, and decorate, and has excellent impact strength and dimensional stability. The product’s UV resistance technology assures long lasting outdoor weathering performance. Makrolon LD is offered with a ten (10) year limited product warranty against breakage.

Applications: Flat and formed sign faces, channel

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Water Absorption 0.15 %
@Time 86400 sec
0.15 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7070ASTM D785
Hardness, Rockwell R 118118ASTM D785
Tensile Strength, Ultimate 65.5 MPa9500 psiASTM D638
Tensile Strength, Yield 62.1 MPa9010 psiASTM D638
Elongation at Break 110 %110 %ASTM D638
Tensile Modulus 2.34 GPa339 ksiASTM D638
Flexural Strength 93.1 MPa13500 psiASTM D790
Flexural Modulus 2.38 GPa345 ksiASTM D790
Compressive Strength 86.2 MPa12500 psiASTM D695
Compressive Modulus 2.38 GPa345 ksiASTM D695
Shear Modulus 0.786 GPa114 ksiASTM D732
Shear Strength 41.4 MPa6000 psiYield; ASTM D732
 68.9 MPa10000 psiBreak; ASTM D732
Izod Impact, Notched 8.54 J/cm
@Thickness 3.17 mm
16.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB
@Thickness 3.17 mm
NB
@Thickness 0.125 in
ASTM D256
Impact Test >= 63.7 J
@Thickness 3.17 mm
>= 47.0 ft-lb
@Thickness 0.125 in
ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.20e+16 ohm-cm8.20e+16 ohm-cmASTM D257
Dielectric Constant  2.96
@Frequency 10 Hz
2.96
@Frequency 10 Hz
ASTM D 150
 3.17
@Frequency 60 Hz
3.17
@Frequency 60 Hz
ASTM D 150
Dielectric Strength 15.0 kV/mm
@Thickness 3.17 mm
381 kV/in
@Thickness 0.125 in
ASTM D149
Dissipation Factor 0.00090
@Frequency 60 Hz
0.00090
@Frequency 60 Hz
ASTM D150
Arc Resistance 10 sec10 secStainless Steel Strip Electrode; ASTM D495
 120 sec120 secTungsten Electrodes; ASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 67.5 µm/m-°C37.5 µin/in-°FASTM D696
Thermal Conductivity 0.195 W/m-K1.35 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 142 °C288 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C270 °FASTM D648
Brittleness Temperature 93.3 °C200 °FASTM D746
Flammability, UL94  V-2
@Thickness 1.52 mm
V-2
@Thickness 0.0598 in
 V-0
@Thickness 5.59 mm
V-0
@Thickness 0.220 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible  27 %
@Thickness 3.00 mm
27 %
@Thickness 0.118 in
B27 white; ASTM D1003
 50 %
@Thickness 3.00 mm
50 %
@Thickness 0.118 in
B48 white; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® SL sheet Polycarbonate
Mocom (ALBIS) ALCOM® LD PC 1000 UV 14107 GY1213-14 PC, special filler, UV stabilized
Mocom (ALBIS) ALCOM® LD PC 1000 UV 14096 GY1200-14 PC, special filler, UV stabilized
Mocom (ALBIS) ALCOM® LD PC 1000 UV 14095 GY1198-14 PC, special filler, UV stabilized
Covestro Makrolon® SL-V sheet Polycarbonate

PCOVEST0838 / 202621

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.