MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gabriel Versamid® 280B75 Polyamide Resin
Categories: Polymer; Thermoset

Material Notes: Versamid® products have proven to be superior coatings resins in many applications, such as industrial maintenance and marine coatings, high-performance architectural paints and high-solids and conventional coatings.

Advantages:

  • Highly resistant to chemical and water corrosion
  • Strong adhesion to a variety of substrates
  • Long pot life
  • Lower sensitivity to substrate impurities
  • Most comply with FDA regulations
Principal Applications: Corrosion resistant primers and topcoats

Comments/Advantages: Polyamide/epoxy adduct 75% by weight in n-butanol or xylene, meets MIL-P-24441

Information provided by Gabriel Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 lb/gal
Solids Content 75 %Theo
Viscosity 4300 - 9000 cP
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 8.0
 
Processing PropertiesOriginal ValueComments
Cure Time 360 minTack Free Time; 3 wet mils
 1440 minThrough Cure; 3 wet mils
Pot Life 360 min60% solids
 
Descriptive Properties
Amine Value240-260[mg KOH/g]
Chemical TypePolyamide Adduct Solution
PHR for Max DSC, Tg87190 EEW Epoxy
Theo Amine Hydrogen Equl Wt.165

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nye Lubricants UniFlor 8310 (472) (UF) Synthetic Oil
Lubriplate 68-P Semi-Synthetic Refrigeration Compressor Oil
Gabriel VERSACURE™ RAC 9948 Aliphatic Amine Curing Agent
Gabriel Phenoxy™ PKHA Solid Polyhydroxylether
Gabriel Gabepro® GPM-888 Mercaptan Epoxy Curing Agent Formulation

PGABR982 / 230683

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.