MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Kennametal Stellite Deloro® N-6 PM cast
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Adhesive wear test data: P/M 0.1, cast 0.1; Abrasive wear test data: P/M 17, cast 35. Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous wear parts. Data provided by the manufacturer, Deloro Stellite Inc.

Product of former Deloro Stellite Inc.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.19 g/cc0.296 lb/in³P/M (98%)
 8.48 g/cc0.306 lb/in³Theoretical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 345345Converted from Rockwell C hardness.
 184
@Temperature 760 °C
184
@Temperature 1400 °F
Converted from Rockwell B hardness
 291
@Temperature 649 °C
291
@Temperature 1200 °F
Converted from Rockwell C hardness
 320
@Temperature 538 °C
320
@Temperature 1000 °F
Converted from Rockwell C hardness
Hardness, Knoop 413413Converted from Rockwell C hardness.
 215
@Temperature 760 °C
215
@Temperature 1400 °F
Converted from Rockwell B hardness
 345
@Temperature 649 °C
345
@Temperature 1200 °F
Converted from Rockwell C hardness
 382
@Temperature 538 °C
382
@Temperature 1000 °F
Converted from Rockwell C hardness
Hardness, Rockwell A 6969Converted from Rockwell C hardness.
 55
@Temperature 760 °C
55
@Temperature 1400 °F
Converted from Rockwell B hardness
 66
@Temperature 649 °C
66
@Temperature 1200 °F
Converted from Rockwell C hardness
 68
@Temperature 538 °C
68
@Temperature 1000 °F
Converted from Rockwell C hardness
Hardness, Rockwell B 110110Converted from Rockwell C hardness. Beyond normal Rockwell B range, for comparison only.
 90
@Temperature 760 °C
90
@Temperature 1400 °F
Hot hardness
Hardness, Rockwell C 3838Hot hardness.
 31
@Temperature 649 °C
31
@Temperature 1200 °F
Hot hardness.
 35
@Temperature 538 °C
35
@Temperature 1000 °F
Hot hardness.
Hardness, Vickers 362362Converted from Rockwell C hardness.
 188
@Temperature 760 °C
188
@Temperature 1400 °F
Converted from Rockwell B hardness
 302
@Temperature 649 °C
302
@Temperature 1200 °F
Converted from Rockwell C hardness
 334
@Temperature 538 °C
334
@Temperature 1000 °F
Converted from Rockwell C hardness
Modulus of Elasticity 200 GPa29000 ksi
 
Component Elements PropertiesMetricEnglishComments
Boron, B 0.60 %0.60 %
Carbon, C 1.1 %1.1 %
Chromium, Cr 29 %29 %
Cobalt, Co <= 3.0 %<= 3.0 %
Iron, Fe <= 3.0 %<= 3.0 %
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo 5.5 %5.5 %
Nickel, Ni 54 %54 %As Remainder
Silicon, Si <= 1.5 %<= 1.5 %
Tungsten, W 2.0 %2.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Deloro® 711 PM cast
Kennametal Stellite Deloro® 716 PM cast
Kennametal Stellite Stellite® 25 Cobalt Chromium Cast Alloy
Kennametal Stellite Deloro® 208 PM cast
Kennametal Stellite Deloro® 40G

NDN6PB / 16113

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.