MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Parker Chomerics CHO-FORM 5532 EMI Shielding Material  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. Cho-Form® 5531 is designed to be robotically dispensed using high pressure dispense equipment

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.02 g/cc3.02 g/cc
 2.80 - 3.30 g/cc2.80 - 3.30 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2626Typical Value; ASTM D2240
 <= 45<= 45ASTM D2240
Tensile Strength at Break >= 0.414 MPa>= 60.0 psiASTM D412
 0.586 MPa85.0 psiTypical Value; ASTM D412
Compression Set 30 %30 %ASTM D395 Method B 22 hrs 85°C
 20 - 45 %20 - 45 %ASTM D395 Method B 22 hrs 85°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.020 ohm-cm0.020 ohm-cmInitial; Chomerics MAT-1002
 <= 0.020 ohm-cm<= 0.020 ohm-cmAged; Chomerics MAT-1002
Shielding Effectiveness >= 70 dB>= 70 dBChomerics TP08
 
Processing PropertiesMetricEnglishComments
Extrusion Rate 5.50 - 7.50 g/min5.50 - 7.50 g/min
Cure Time  2.00 min
@Temperature 65.0 °C
0.0333 hour
@Temperature 149 °F
85% RH
 3.00 min
@Temperature 30.0 °C
0.0500 hour
@Temperature 86.0 °F
85% RH
 
Descriptive Properties
FillerAg/Cu
ResinOne Part Silicone
Shear Adhesion N/cm VMin12

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics CHO-FORM 5526 EMI Shielding Material
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam
Parker Chomerics MESH STRIP™ (Elastomer Core) Wire Mesh EMI Gasket Selection Guide
Parker Chomerics CHO-VER SHIELD™ EMI Shielding Covers with Over-Molded Conductive Elastomer Gasket
Overview of materials for Epoxy, Thermally Conductive

PCHOME086 / 28308

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.