MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Algoflon® D 2510 F Polytetrafluoroethylene (PTFE)  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); PTFE Powder

Material Notes: Algoflon® D 2510 F is a PFOA-free white aqueous PTFE dispersion. It is designed for impregnation processes and is particularly recommended for production of fabrics and laminates. Algoflon® D 2510 F exhibits excellent wetting properties and high shear stability. Algoflon® D 2510 F has low foaming behavior and is optimized for basecoat passes.

Features: Good Chemical Resistance; High Heat Resistance; Low Friction

Uses: Coating Applications; Impregnation Applications

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.51 g/ccASTM D4441
Particle Size 240 µm
pH >= 9.0ASTM D4441
Brookfield Viscosity 25 cPASTM D4441
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
ColorWhite
FormLatex
Non Ionic Surfactant3%on the mixture, ASTM D4441
PTFE Content60%on the mixture, ASTM D4441

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Catalyst CAT 10 Polyolefin
Syensqo (Solvay Specialty Polymers) Polidan® EC/51 Polyethylene, Crosslinked (XLPE)
Syensqo (Solvay Specialty Polymers) Polidan® T/A Polyethylene, Crosslinked (XLPE)
Syensqo (Solvay Specialty Polymers) Polidan® TUX 100 Polyethylene, Crosslinked (XLPE)
Overview of materials for Polytetrafluoroethylene (PTFE) Powder

PSOL8Y6913 / 176644

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.