MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Meyors Chemical Vulca Pellet DM-8
Categories: Other Engineering Material

Material Notes: Product Code: MSHQD-AC070-02 GT
Chemical Name: Vulca Pellet DM-8
Trade Name: Vulca Pellet DM-8
CAS No.: 120-78-5
Molecular Formula: C14H8N2S4

Typical Properties: A proprietary pre-dispersed 80% Dibenzothiazyl disulphide in a 20% electrometric (EPDM)/processing aids binder. (electrometric binder can be SBR or EPDM).

Recommended Applications: The active ingredient of Vulca Pellet DM-80 is an all purpose accelerator and is the first delayed action accelerator in history. Vulca Pellet DM-80 used by itself, gives good processing safety, intermediate cure rate, flat curve and very good aging resistant Vulcan sate. It prevents scorching in combination with activated dithiocarbamate. Vulca Pellet DM-80 can be activated by thiuram, dithiocarbamates and aldehyde-amines.

Information provided by Meyors Chemical INC Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/cc
Mooney Viscosity <= 30
@Temperature 100 °C
ML 1+4
Molecular Weight 332 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 165 °CInitial
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 1.0 %of active DM
 
Descriptive Properties
AppearanceBeige granule
Assay content>80%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMEYORS008 / 316590

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.