MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Tellurium-Bearing Copper Alloy, UNS C14510, H55 Temper, Tube
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Fabrication Properties: Excellent Suitability - Soldering; Good Suitability – Brazing, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Fair Suitability - Oxyacetylene Welding, Gas Shielded Arc Welding, Butt Weld

Common Fabrication Processes: Cold - Drawing, machining, moderate cold heading; Hot - Extrusion, forging (closed die only)

Typical Uses: Fire Protection; Electrical Connectors; Motor Parts; Soldering Copper; Switch Parts; Transistor Bases; Forgings; Furnace Brazed Articles; Screw Machine Products; Wielding Torch Tips; Plumbing Fittings; Sprinkler Heads

Applicable Specifications: Bar – ASTM B301/B301M; Rod– ASTM B301/B301M; Shapes – ASTM B301/B301M; Wire – ASTM B301/B301M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 3535
Tensile Strength 276 MPa40000 psi
Tensile Strength, Yield 221 MPa32000 psi0.2% Offset
Elongation at Break 20 %20 %
Tensile Modulus 117 GPa17000 ksi
Modulus of Rigidity 44.1 GPa6400 ksi
Poissons Ratio 0.330.33Calculated
Machinability 85 %85 %
Forgeability 65 %65 %
Shear Strength 165 MPa24000 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.1 µm/m-°C
@Temperature 20.0 - 100 °C
9.50 µin/in-°F
@Temperature 68.0 - 212 °F
 17.5 µm/m-°C
@Temperature 20.0 - 200 °C
9.70 µin/in-°F
@Temperature 68.0 - 392 °F
 17.8 µm/m-°C
@Temperature 20.0 - 300 °C
9.90 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Thermal Conductivity 29.5 W/m-K205 BTU-in/hr-ft²-°F
Melting Point 1051 - 1075 °C1924 - 1967 °F
Solidus 1051 °C1924 °F
Liquidus 1075 °C1967 °F
Annealing Point 427 - 649 °C800 - 1200 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 760 - 871 °C1400 - 1600 °FStress Relief
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 99.85 %>= 99.85 %
Phosphorus, P 0.010 - 0.030 %0.010 - 0.030 %
Tellurium, Te 0.30 - 0.70 %0.30 - 0.70 %
Zinc, Zn <= 0.050 %<= 0.050 %
 
Descriptive Properties
Cold Work (%)15
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC14510x6 / 291540

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.