MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LG Chemical LUPOY 1301EP-30 Polycarbonate, Injection Molded
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Introduction: LUPOY PC 1301EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.

Main Characteristics: Very low viscosity, Good mold release

Applications: DVD security boxes, Mobile phone keypads, Thin components, Packaging applications

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Absorption 0.15 %
@Time 86400 sec
0.15 %
@Time 24.0 hour
ASTM D570
Moisture Absorption at Equilibrium 0.32 %0.32 %50% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 30 g/10 min
@Load 1.20 kg,
Temperature 300 °C
30 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 61.0 MPa8850 psiASTM D638
Tensile Strength, Yield 60.0 MPa8700 psi50mm/min; ASTM D638
Elongation at Break 150 %150 %ASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Tensile Modulus 2.34 GPa339 ksiASTM D638
Flexural Strength 96.0 MPa13900 psiASTM D790
Flexural Modulus 2.41 GPa350 ksiASTM D790
Izod Impact, Notched 6.94 J/cm
@Thickness 3.20 mm
13.0 ft-lb/in
@Thickness 0.126 in
0.25 mm notch; ASTM D256
Izod Impact, Unnotched NBNBASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+17 ohm-cm2.00e+17 ohm-cmdry; ASTM D 257
Dielectric Constant 3.0
@Frequency 60 Hz
3.0
@Frequency 60 Hz
ASTM D 150
Dielectric Strength 16.5 kV/mm420 kV/inASTM D 149
Dissipation Factor 0.0010
@Frequency 60 Hz
0.0010
@Frequency 60 Hz
ASTM D 150
Comparative Tracking Index 250 V
@Thickness 2.00 mm
250 V
@Thickness 0.0787 in
IEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 68.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F
@Temperature -40.0 - 180 °F
ASTM D 696
Hot Ball Pressure Test >= 125 °C>= 257 °FIEC 598-1
Deflection Temperature at 0.46 MPa (66 psi) 139 °C282 °FAnnealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °C252 °FUnannealed; ASTM D648
 136 °C277 °FAnnealed; ASTM D648
Vicat Softening Point 144 °C
@Load 5.00 kg
291 °F
@Load 11.0 lb
50°C/h; ASTM D1525
Flammability, UL94  V-2
@Thickness 0.500 mm
V-2
@Thickness 0.0197 in
 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
 V-2
@Thickness 2.50 mm
V-2
@Thickness 0.0984 in
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
Oxygen Index 26 %26 %ASTM D 2863
Glow Wire Test 850 °C
@Thickness 2.00 mm,
Time 5.00 sec
1560 °F
@Thickness 0.0787 in,
Time 0.00139 hour
IEC 695-2-1
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ASTM D542
Haze 0.70 - 1.5 %0.70 - 1.5 %ASTM D1003
Transmission, Visible 89 %89 %ASTM D1003
 
Descriptive Properties
Average Extent of Burning25 mmASTM D 635

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLHCHEM9720 / 239244

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.