MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Inov Chem DZJ-02A/02B Integral Skin Foam System
Categories: Polymer

Material Notes: Applications: This kind of product is widely used for making armrest, steering wheel, seat cushion, etc.

Characteristics: DZJ-A is type of blend Polyol combined with base polyol, cross-linking agent, blowing agent, cat. and some other agent. DZJ-B is isocynate combined with MDI. & modified MDI. The system is suitable to produce integral skin foam which without TDI, eco-friendly, low smell, suitable hardness.

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.120 - 0.150 g/cc0.120 - 0.150 g/ccFRD
 0.350 - 0.400 g/cc0.350 - 0.400 g/ccOverall Density
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 70 - 8070 - 80
 
Processing PropertiesMetricEnglishComments
Mold Temperature 40.0 - 50.0 °C104 - 122 °F
 
Descriptive Properties
Demolding Time3-4 min
Ratio100/50-100/55Polyol/Iso

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PINOVCHM212 / 312741

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.