MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Chevron Phillips K-Resin® KR10 Styrene-Butadiene Copolymer, Film Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.

Customer Benefits: This SBC is easily processed on blown film or cast film equipment to give tough, high clarity film. Film produced has excellent clarity, good toughness, excellent stiffness, good heat sealability, high surface gloss, and high permeation. Has a puncture value of 1.2 J as per ASTM D3763, a 99 % crease retention as per TAPPI T446-B, and a 0.6 g mm/m^2 24h moisture vapor transmission as per ASTM F1249 at 23°C. Film shrinkage is 67% MD and 48% TD.

Applications: Major applications include medical packaging, produce packaging, skin packaging, twist wrap, lidstock film, labeling film, decorative films, industrial films, shrink wrap, overwrap film, barrier film, and tamper evident packaging

Processing Recommendations:
Blown Film: Melt Temperature, 166-193°C recommended. Cast Film: Melt Temperature, 193-216°C recommended. High shear and restrictive type screws tend to degrade the melt.

Specification Data: FDA Regulation 21 CFR 177.1640. Suitable for food contact. EEC Directive 90/128/EEC and all its amendments. USP Class VI-50. UL 94HB.

Data provided by Chevron Phillips Chemical Company LP.

Ineos Styrolution acquired the K-Resin® product line from Chevron Phillips Chemical Company in 2016. This grade was previously discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccASTM D792
Moisture Vapor Transmission 0.600 cc-mm/m²-24hr-atm@ 23°C; ASTM F1249
Oxygen Transmission 173 cc-mm/m²-24hr-atmASTM D3985
Melt Flow 7.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 26.0 MPa2 in per min; ASTM D882
Film Tensile Strength at Yield, TD 16.0 MPa2 in per min; ASTM D882
Film Elongation at Break, MD 65 %ASTM D882
Film Elongation at Break, TD 175 %ASTM D882
Secant Modulus, MD 1.275 GPaat 1%; ASTM D882
Secant Modulus, TD 0.883 GPaat 1%; ASTM D882
Elmendorf Tear Strength, MD 0.550 g/milASTM D1922
Elmendorf Tear Strength, TD 0.690 g/milASTM D1922
Dart Drop Test 345 g26 in; ASTM D1709
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Haze 2.0 %ASTM D1003
Gloss 129 %45°; ASTM D2457
Transmission, Visible 99 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 166 - 193 °CBlown Film
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
USP Class VI Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips K-Resin® BK11 Styrene-Butadiene Copolymer, Injection Molding Grade
Chevron Phillips K-Resin® BK15 Styrene-Butadiene Copolymer, Injection Molding Grade
Chevron Phillips K-Resin® CK02 Styrene-Butadiene Copolymer, Blow Molding Grade
Chevron Phillips K-Resin® BK18 Styrene-Butadiene Copolymer
Chevron Phillips K-Resin® BK13 Styrene-Butadiene Copolymer, Injection Molding Grade

PCHEVK70 / 20287

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.