MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Lubrizol Pellethane® 2363-65D Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Feature: USP Class VI

Available in Americas, Europe, Middle East, Africa, India and Asia

Data provided by Lubrizol

Lubrizol acquired the Pellethane product line from Dow in 2009.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0080 - 0.0090 cm/cm0.0080 - 0.0090 in/inASTM D955
Melt Flow 40 g/10 min
@Load 5.00 kg,
Temperature 224 °C
40 g/10 min
@Load 11.0 lb,
Temperature 435 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6262ASTM D2240
Tensile Strength, Ultimate 44.5 MPa6450 psiASTM D412
Elongation at Break 450 %450 %ASTM D412
50% Modulus 16.2 MPa
@Strain 50 %
16.2 MPa
@Strain 50 %
ASTM D412
100% Modulus 20.0 MPa
@Strain 100 %
2900 psi
@Strain 100 %
ASTM D412
300% Modulus 34.5 MPa
@Strain 300 %
5000 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.221 GPa32.1 ksiASTM D790
Tear Strength 193 kN/m1100 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 105105H22 Wheel; ASTM D1044
Compression Set  30 %
@Temperature 25.0 °C,
Time 79200 sec
30 %
@Temperature 77.0 °F,
Time 22.0 hour
ASTM D395
 35 %
@Temperature 70.0 °C,
Time 79200 sec
35 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Tensile Set 50 %50 %Elongation set after break; ASTM D412
 
Thermal PropertiesMetricEnglishComments
CTE, linear 104 µm/m-°C
@Temperature -80.0 - -30.0 °C
57.8 µin/in-°F
@Temperature -112 - -22.0 °F
ASTM D696
Vicat Softening Point 107 °C225 °F120°C/hr, 9.8N; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 221 °C399 - 430 °FExtrusion
 210 - 227 °C410 - 441 °FMolding
Mold Temperature 16.0 - 60.0 °C60.8 - 140 °F
Drying Temperature 99.0 - 110 °C210 - 230 °Fair dew point <-40°C
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Pellethane® 2363-75D Thermoplastic Polyurethane Elastomer
Lubrizol Pellethane® 2363-55D Thermoplastic Polyurethane Elastomer
Lubrizol Pellethane® 2363-80A Thermoplastic Polyurethane Elastomer
Lubrizol Pellethane® 2363-55DE Thermoplastic Polyurethane Elastomer
Lubrizol Pellethane® 2363-90A Thermoplastic Polyurethane Elastomer

PDW286a / 138246

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.