MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL™ Resin PX1860 Polyphenylene Ether + PS (PPE+PS) (Americas)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL PX1860 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR additives to achieve a V1 UL94 rating at 1.5 mm with a specific density of 1.1 g/cm^3. NORYL PX1860 may be an excellent material candidate for Flat Panel TV enclosure applications requiring good rheological properties, heat resistance, hydrolysis resistance, low density and thin wall flame resistance.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Moisture Absorption 0.0200 %0.0200 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.13 %0.13 %ISO 62-1
Viscosity 34 cP
@Load 2.16 kg,
Temperature 280 °C
34 cP
@Load 4.76 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 49.0 MPa7110 psi50 mm/min; ASTM D638
Tensile Strength, Yield 52.0 MPa7540 psi50 mm/min; ASTM D638
Elongation at Break 7.3 %7.3 %50 mm/min; ASTM D638
Elongation at Yield 3.6 %3.6 %50 mm/min; ASTM D638
Tensile Modulus 3.14 GPa455 ksi50 mm/min; ASTM D638
Flexural Strength 98.0 MPa14200 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.77 GPa402 ksi1.3 mm/min, 50 mm span; ASTM D790
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+16 ohm-cm4.00e+16 ohm-cmASTM D257
 4.00e+16 ohm-cm4.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmASTM D257
 1.00e+14 ohm1.00e+14 ohmROA; IEC 60093
Comparative Tracking Index 250 V250 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
UL RTI, Electrical 65.0 °C149 °FUL 746B
UL RTI, Mechanical with Impact 65.0 °C149 °FUL 746B
UL RTI, Mechanical without Impact 65.0 °C149 °FUL 746B
Flammability, UL94 V-1
@Thickness >=1.50 mm
V-1
@Thickness >=0.0591 in
UL 94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82446 / 290393

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.