Description: Partially recycled PA6 30% glass-fiber-reinforced injection molding grade. Heat stabilized. Black color. This material has been developed to reduce its environmental impact compared to first-choice grades, through the recovery of post-consumer (end-of-life) components previously classified as waste. Suitable for parts requiring high stiffness and good mechanical resistance. Processing: Injection Molding Delivery Form: Granules Additives: Release agent Special Characteristics: Heat stabilized or stable to heat Sustainability: Pre-consumer Recycling Industries: Automotive, Consumer Industry Goods, Transportation Regional Availability: Europe Information provided by Radici Group |