MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
ITW Insulcast® 987 Epoxy Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. INSULCAST 987 is a semi-flexible, potting compound that exhibits excellent electrical and physical properties over a wide range of temperatures.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.37 g/ccuncured
 1.41 g/ccuncured
Viscosity 50000 cPUncured. Part B; ASTM D2393
 60000 cPUncured, mixed; ASTM D2393
 80000 cP
@Temperature 23.0 °C
Part A; ASTM D2393
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Constant 4.9
@Frequency 1000 Hz
cured; ASTM D150
Dielectric Strength 375 V/milASTM D149
Dissipation Factor 0.050
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 45.0 µm/m-°C
Thermal Conductivity 2.90 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 155 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Pot Life >= 2800 min
@Temperature 23.3 °C
Shelf Life 12.0 Month
 
Descriptive Properties
Colorneutralpart A, uncured
 neutralpart B, uncured
Mix Ratio by weight2 to 3Part A: Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWIN9104 / 239614

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.