MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SEKISUI SPI ALLEN® 8150SM PC/ABS Sheet
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: ALLEN® 8150SM is a general purpose PC/ABS with high impact strength and high heat deflection.

ALLEN® 8150SM meets the requirements of Federal Motor Vehicle Safety Standard No. 302 (FMVSS 302).

Suggested Application:

  • Vehicle Interior Trim
  • Covers and Housings
  • Vehicle Exteriors (painted)
  • Instrument Panels
Features:
  • Custom color matching
  • Good forming properties
  • Edge trim easily used for future orders
  • High heat deflection temperature
  • High gloss finish
  • Meets many automotive specification

Information provided by SEKISUI KYDEX, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
Water Absorption 0.170 %
@Time 86400 sec
0.170 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 111111ASTM D785
Tensile Strength 48.0 MPa6960 psiASTM D638
Tensile Modulus 2.096 GPa304.0 ksiASTM D638
Flexural Strength 80.0 MPa
@Strain 5.00 %
11600 psi
@Strain 5.00 %
ASTM D790
Flexural Modulus 2.23 GPa323 ksiASTM D790
Compressive Yield Strength 59.2 MPa8590 psiASTM D695
Bearing Yield Strength <= 228.2 MPa<= 33100 psiASTM D953
 27.9 MPa
@Strain 4.00 %
4050 psi
@Strain 4.00 %
ASTM D953
Shear Strength 54.0 MPa7830 psiASTM D732
Izod Impact, Notched 5.239 J/cm9.815 ft-lb/inASTM D256
Gardner Impact 50.1 J37.0 ft-lbDrop Dart Impact, GE; ASTM D5420
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 21.7 kV/mm551 kV/inoil; ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 77.0 µm/m-°C42.8 µin/in-°FASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 129 °C264 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 118 °C244 °Fannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSEKIS526 / 325266

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.